| MOQ: | 8000 s.q.m |
| Price: | $0.1/s.q.m for quantities less than 100,000 s.q.m on FOB Shanghai basis |
| Standard Packaging: | EPE film + PE wrap + Processed wooden pallet |
| Delivery Period: | within 15 days depends on the reserve of raw materials |
| Payment Method: | T/T,L/C |
| Supply Capacity: | 100000 kg per week |
| Test Item | Unit | Standard Index | Test Result | Test Method |
|---|---|---|---|---|
| Measured Value | μm | M ± 2% | 23.05 | ASTM D-374 |
| Tensile Strength (MD) | Mpa | ≥180 | 188 | ASTM D-882 |
| Tensile Strength (TD) | Mpa | ≥200 | 224 | ASTM D-882 |
| Elongation @ Break (MD) | % | ≤200 | 133 | ASTM D-882 |
| Elongation @ Break (TD) | % | ≤200 | 123 | ASTM D-882 |
| Elasticity Modulus (MD) | Mpa | ≥3500 | 4773 | ASTM D-882 |
| Elasticity Modulus (TD) | Mpa | ≥3500 | 4646 | ASTM D-882 |
| Thermal Shrinkage (MD) | % | ≤1.5 | 1.70 | 150℃/30min |
| Thermal Shrinkage (TD) | % | ≤0.5 | -0.16 | 150℃/30min |
| Haze | % | ≤5.0 | 5.23 | ASTM D-1003 |
| Light Transmittance | % | ≥88 | 91.5 | ASTM D-1003 |
| Glossiness (45°) | % | ≥80 | 95.6 | ASTM D-2457 |
| Clarity | % | ≥90 | 92.6 | ASTM D-1003 |
| Friction Co-efficiency (μs) | - | ≤0.65 | 0.108 | ASTM D-1894 |
| Friction Co-efficiency (μk) | - | ≤0.50 | 0.102 | ASTM D-1894 |
| Coating Weight | g/㎡ | 0.075~0.2 | 0.182 | FTM7 |
| Release Force (after 20min.) | g/25mm | 5~15 | 12.269 | FTM 1 (w/out briquette) |
| Subsequent Adhesion Rate | % | ≥88 | GB/T 25256-2010 |
|
|
| MOQ: | 8000 s.q.m |
| Price: | $0.1/s.q.m for quantities less than 100,000 s.q.m on FOB Shanghai basis |
| Standard Packaging: | EPE film + PE wrap + Processed wooden pallet |
| Delivery Period: | within 15 days depends on the reserve of raw materials |
| Payment Method: | T/T,L/C |
| Supply Capacity: | 100000 kg per week |
| Test Item | Unit | Standard Index | Test Result | Test Method |
|---|---|---|---|---|
| Measured Value | μm | M ± 2% | 23.05 | ASTM D-374 |
| Tensile Strength (MD) | Mpa | ≥180 | 188 | ASTM D-882 |
| Tensile Strength (TD) | Mpa | ≥200 | 224 | ASTM D-882 |
| Elongation @ Break (MD) | % | ≤200 | 133 | ASTM D-882 |
| Elongation @ Break (TD) | % | ≤200 | 123 | ASTM D-882 |
| Elasticity Modulus (MD) | Mpa | ≥3500 | 4773 | ASTM D-882 |
| Elasticity Modulus (TD) | Mpa | ≥3500 | 4646 | ASTM D-882 |
| Thermal Shrinkage (MD) | % | ≤1.5 | 1.70 | 150℃/30min |
| Thermal Shrinkage (TD) | % | ≤0.5 | -0.16 | 150℃/30min |
| Haze | % | ≤5.0 | 5.23 | ASTM D-1003 |
| Light Transmittance | % | ≥88 | 91.5 | ASTM D-1003 |
| Glossiness (45°) | % | ≥80 | 95.6 | ASTM D-2457 |
| Clarity | % | ≥90 | 92.6 | ASTM D-1003 |
| Friction Co-efficiency (μs) | - | ≤0.65 | 0.108 | ASTM D-1894 |
| Friction Co-efficiency (μk) | - | ≤0.50 | 0.102 | ASTM D-1894 |
| Coating Weight | g/㎡ | 0.075~0.2 | 0.182 | FTM7 |
| Release Force (after 20min.) | g/25mm | 5~15 | 12.269 | FTM 1 (w/out briquette) |
| Subsequent Adhesion Rate | % | ≥88 | GB/T 25256-2010 |